Material | 50CrMo Precision Forged Alloy Steel |
---|---|
Coating | 60-80μm, American Praxair Super Hard 1342 Tungsten Cabide Powder |
Width | 2200mm×Φ340mm |
Heating Treatment | Intermediate Frequency Quenching |
Hardness | >HRC58 After Hardening |
Material | 50CrMo Precision Forged Alloy Steel |
---|---|
Coating | 60-80μm American Praxair Super Hard 1342 Tungsten Cabide Powder |
Heating Treatment | Intermediate Frequency Quenching |
Harden Layer | 8-12mm |
Hardness | >HRC58 After Hardening |
Material | 50CrMo Precision Forged Alloy Steel |
---|---|
Coating | 60-80μm American Praxair Super Hard 1342 Tungsten Cabide Powder |
Width | 1700mm×330mm |
Heating Treatment | Intermediate Frequency Quenching |
Hardness | >HRC58 After Hardening |
Material | 50CrMo Precision Forged Alloy Steel |
---|---|
Coating | 60-80μm American Praxair Super Hard 1342 Tungsten Cabide Powder |
Size | 2400mm*408mm |
Micro Hardness | HV1250-1400 |
Heating Treatment | Intermediate Frequency Quenching |
Material | 50CrMo Precision Forged Alloy Steel |
---|---|
Coating | 60-80μm American Praxair Super Hard 1342 Tungsten Cabide Powder |
Size | 2100mm×360/380mm |
Heating Treatment | Intermediate Frequency Quenching |
Hardness | >HRC58 After Hardening |
Material | 50CrMo Precision Forged Alloy Steel |
---|---|
Coating | American Praxair Super Hard 1342 Tungsten Cabide Powder |
Coating Thickness | 60-80μm |
Size | 1800mm×300mm |
Heating Treatment | Intermediate Frequency Quenching |
Material | 50CrMo Precision Forged Alloy Steel |
---|---|
Coating | Hard Chrome 60-80μm |
Heating Treatment | Intermediate Frequency Quenching |
Hardness | >HRC58 After Hardening |
Harden Layer Depth | 8-12mm |
Material | 50CrMo Precision Forged Alloy Steel |
---|---|
Coating | Hard Chrome 60-80μm |
Size | 1600mm×320mm |
Steel Wall Thickness | ≥70mm |
Heating Treatment | Intermediate Frequency Quenching |
Material | 50CrMo Precision Forged Alloy Steel |
---|---|
Coating | 60-80μm American Praxair Super Hard 1342 Tungsten Cabide Powder |
Heating Treatment | Intermediate Frequency Quenching |
Harden Layer | 8-12mm |
Hardness | >HRC58 After Hardening |
Material | 50CrMo Precision Forged Alloy Steel |
---|---|
Coating | 60-80μm American Praxair Super Hard 1342 Tungsten Cabide Powder |
Width | 2500mm×Φ295/346mm |
Heating Treatment | Intermediate Frequency Quenching |
Hardness | >HRC58 After Hardening |